The polydispersity
coefficient values of GP-LRS3, MP-LRS3 and UP-LRS3 were 1.249,
1.298 and 1.247, respectively. This indicated that all samples had
narrower molecular weight distribution. Luckett (2012) reported
the relatively appropriate degree of polymerization (DP) was
benefit for the formation of double helices and crystallization.