The as-synthesized carbon products containing amorphous carbon admixtures were further purified from metal oxide
template by boiling in 10% solution of hydrochloric acid for 4 h with ultrasonication. After that the materials were washed with distilled water until neutral pH, annealed in the muffle furnace for 4 h at 330 C and then dried in vacuum oven at 120 C.