Chelation stages (Q) were performed at pulp consistencies of 10% for one hour at 75 °C. At the beginning of the treatment, a 0.5% charge of EDTA was applied to the pulp, and the pH was adjusted to 5 using H2SO4. After 60 minutes of treatment, the pulp was washed as described previously