Although it may occasionally occur because of a severe process breakdown, delamination and blistering occurs as a result of an inherent weakness of the material. Either condition represents a breakdown in the cohesive strength of the composite laminate and the internal openings that develop can mechanically weaken in the final product and also provide undesirable conductive paths between circuit elements.