The obtained white solid was recovered by vacuum filtration, washed several times with distilled water and air-dried overnight at 80 C. Organic molecules occluded in the mesopores were removed by direct calcination at 500 C with air flow for 6 h. The small pore size silica support (SBA-15-1) was synthesized without any hydrothermal treatment.