2.1. Wood Filler
Pine wood flour is used as a reinforcing material in this study which is collected from the local Kanpur saw
mill G.T.Road The fresh sawdust of pine wood received is dried at 103°C for 24 h to a moisture content of
about 2-3% and then grounded to finer flour by using a sieve analysis. The sieve analysis found that most of
the wood particles remained in the 35-45 mesh sizes with corresponding particle diameter ranging between
0.2 and 0.5 mm (200um