The strength value by new measuring method is not bad result as same SHP1055.
But, we found terminal defect at 0760-1R0 winding with only 4N Karage tension.
Please confirm the 2 items as below;
1. Different point (changing point) of terminal bonding process between your test and 1R0 trial.
2. Terminal bonding with 3 point adhesive (below picture) and terminal strength.