It must be very important to concentrate on the PLA/NR system with the content of 90/10 where the
elongation at break is very much enhanced. In this particular composition, there was plastic deformation
with whitening zone occurring during tensioning. It was clearly shown by the elongated deformed plastic
on the fractured surface shown in Fig. 7. But the rest compositions seem to show no plastic deformation.