Two experiments were carried out to show the influence of process parameters to the damage behaviour of the surface. In the experiments, a rod (D1 and a length of 120 mm) made of 37MnSi5 was used as workpiece, the tool was made of a ball bearing SKF 7301B.JP with 8 balls (Fig. 2).