X-ray diffractometry and differential scanning calorimetry (DSC) elucidated that all the initially amorphous PLA films remained amorphous, even after autocatalytic hydrolysis for 16 (PDLLA film) and 24 (non-blended PLLA and PDLA films,PLLA/PDLA(1/1)blend film) months.