This composite was used in a second step to obtain SiC at a temperature of 1500 C, in argon atmosphere. The experimental setup used a Pyrex glass spherical vessel designed to work with concentrated solar power and controlled atmospheres.
This composite was used in a second step to obtain SiC at a temperature of 1500 C, in argon atmosphere. The experimental setup used a Pyrex glass spherical vessel designed to work withconcentrated solar power and controlled atmospheres.