The further increase of the composite PCM volume replacement level from 50% to 100% leads to further unclear density reduction.
Due to the high water absorptivity of the expanded vermiculite, LW-TESCC-100 has much worse workability and thus requires longer vibration assistant during the specimen preparation.
This could result in more compacted microstructure of LW-TESCC-100 and the observed slight further density reduction.