The results on day 10 PI showed that healing was well underway in both the treated
and untreated groups considering wound contraction and cell proliferation, which are
shown in Tables 1 and 2. As shown in Fig. 1, the biomechanical properties of the treated
and untreated samples were almost similar and did not show a signifi cant difference on
day 10 PI, moreover, both were inferior to their intact contra-lateral skin samples.