According to this criteria, storage modulus at the reference
temperature of 0 C (G0
Tref¼0 C) and damping factor at the reference
temperature of 8 C (tan dTref¼8 C) were selected in order
to facilitate the development of accurate and valid kinetic models.
Storage modulus at the test reference temperature of 0 C was
plotted against storage time for each storage temperature