Dear K’ Mana.
Today I send GX to LET size 11 Kva 5 Pcs but all in lot incomplete polishing. PASS QC test adhesion by attaching 3 M tape and pulling 100% ( 3 point). I convinced for this lot not problem. I will start use sticker OK for raw mat 12 Pcs in stock You can sent GX reject 2 Pcs with transport.
In process ;
1.) internal process we discuss with QC following your requirement revise WI.
- Created surface pre-treatment
- Created time inspect surface before send to next process.
- Final inspect test adhesion use tape and pulling 3 point.
All process we will check and test if completed I send WI to you consider.