At the location of P5, i.e. the edge of the test-piece, the effective strain is less than 0.2. With an increasing time, relative densities at these locations are increased at different rate, which has the correlation with the effective strain and triaxiality: a smaller negative value of triaxiality and a larger effective strain can prompt the porosity elimination with a higher rate.