The weight ratio of hydrazine to GO was about 7:10. After being vigorously shaken or
stirred for a few minutes, the vial was put in a water bath (~95 oC) for 1 h. Unless specifically stated,
graphene dispersions prepared according to the above procedure were used for further
characterization and film fabrication in this work