Design Guide and in various articles in this chapter. With an unsealed joint, contraction
under cooler temperatures allows joint cavities to open up and become filled with sand,
stone, and other incompressible material. When warmer temperatures try to expand the
length of the pavement, the joints are unable to close, compressive stresses develop, and
spalling may result