Even though a high cooling rate is achieved during the atomization
process, image analysis performed on SEM micrographs of
cross sections of Cu–23.7Ag powder grains (Fig. 3c) shows a
proportion of Ag-rich phase (white color) close to 23 wt%, which is
in line with the equilibrium composition.