The resulting mixture was heated at 70 to 80°C under vigorous stirring to dissolve the PVP polymer, followed by cooling down to room temperature to form a gel electrolyte
The resulting mixture washeated at 70 to 80°C under vigorous stirring to dissolve the PVP polymer, followed by coolingdown to room temperature to form a gel electrolyte