In addition, the samples
treated at 600 MPa for 5 min at 40 °C showed no changes in the
X-ray diffraction patterns, compared to the raw materials and the untreated
samples. Only a slight reduction of their scattering intensities
was observed, indicating few changes in terms of starch crystallinity