All consumer packs were produced according acceptable level of surface tension and it was not found any tearing during packing process
or at final inspection released by QA. Based on returned sample received from market, it revealed that consumer packed was went to shrink
wrap process cause too much tight on consumer packs' surface and tearing finally. In addition, we notice melt of hang tag