2.4. Preparation of PVA fiber paper reinforced with CNCC
2 g of PVA fibers was formulated into 1000 ml PVA suspensions,
then were beat and dispersed in a disintegrator (total number of
revolution is 15,000 r).
The remaining experimental procedures were the same as those
of the preparation of cellulosic paper.