However, the present investigation revealed that the compressive strength of concrete specimens developed using GRP waste powder was found to be higher than that of the normal requirement for precast concrete walling element (>5 MPa), lightweight concrete (>5 MPa), and concrete blocks (7–35 MPa) and confirmed the potential applications of GRP waste as an additive or filler in concrete