I sent report plating Process : EK-757 Alkaline Zinc Nickel test to you. and during Salt spray test : finish report about in the middle August 2015 (960 hrs.)
I sent report plating Process : EK-757 Alkaline Zinc Nickel test to you.and during Salt spray test : finish report about in the middle August 2015 (960 hrs.)