Vulcanizates with greater reclaim content required less time to reach an equilibrium.
At the equilibrium state, the degree of swelling of the NR vulcanizates reduced with increasing reclaim content. The sample with 80% reclaimed rubber was seen to reach the equilibrium first, and exhibited the lowest value of toluene uptake.
The decrease in Qa due to the