three composite samples were taken to the laboratory where they were air-dried, passed through a 2.0 mm sieve and homogenised in a mortar .Each sample was divided into 3 sub sample and 0.5 g was acid digested using a standard protocol ( Thompson,2009)prior to ICP-OES analysis.