Alkali fusion and silicate extraction were then conducted based on the procedure reported by Kumar et al.. Bottom ash was mixed with NaOH powder at a 1:1.2 weight ratio. It was then fused at 600 ◦C for 1 h. The fused mixture was cooled to room temperature, ground to fine powder, and finally mixed with water at a weight ratio of 1:4.