Because of the difference of adsorbed water and interlayer water in the two samples, the weight loss of stage one in the hybrid is about 8.9%more than that of pure LDH. So the weight percentage of rGO in NiMn LDH/rGO can be thus calculated to be 4.5%, well consistent with the result measured by the weights of initial GO and the final composite product