Fracture veins/striations and clam shell markings of the fracture morphologies displays a fatigue fracture features and indicate the propagation direction of the fatigue crack. On other hand dendrite morphology of the surface indicates instantaneous fracture features mainly due to last
stage of the fracture process or aroused by hitting the initial broken blade at high rotating speed.