(3) The shear stress on the surface (zo10 μm) is greater than that
in the subsurface (50 μmozo100 μm), and the original source
of crack is formed close to the surface firstly. Micro-pitting
appears before macro-pitting happened at the surface. Once
micro-pitting forms, surface stress grows larger on the subsurface,
accelerating the expansion of pitting.