This is especially obvious with preheating and processing at temperatures well above the
softening temperature of the lignin, which for spruce chips is at 125–145 °C at the processing
conditions in question. The final pulp quality is controlled by the energy input to the mechanical
processing of the fibre material. The intensity and the speed of the processing have a large influence
on the final properties of the fibres as well.