Following UHP treatment at
600 MPa, the mean volume diameter was approximately
30.22 lm. Additionally, d (0.1), d (0.5), and d (0.9) increased at
400 MPa; d (0.9) increased from 16.79 lm (native starch) to
58.95 lm (UHP-treated starch), indicating the increased number
of large granules. These results were in agreement with the results
reported by Liu et al.