Solidification caused by cooling results in the forming of frozen layer near the cavity surface. With the increasing of time, the frozen ratio increases. The increase of frozen ratio not only reduces the cross-section along the flow path, but also increases the flow resistance and sprue pressure. Furthermore, the residual stress and flow-induced orientation will be affected.