was evaluated by compression at the
center of cookies 50 mm diameter and 3 mm thickness to 80% of the
original height at a test speed of 1.0 mm/s after cookies were
brought to room temperature for 1 h. The first peak force was
recorded as hardness. All measurements were repeated seven
times