3.5. Effect of MP on microstructure
Fig. 10 shows PLM images taken at the start of crystallization at
20 °C. The sample containing 1% MP had a similar microstructure as
PO but, from a concentration of 2% MP onwards, a coarser crystal structure
could be seen as more MP was added