A possible explanation of the lower
collection efficiency could be a completely different morphology due to over-firing by an excessively high sintering
temperature and decreased Brownian diffusion due to the
increased pore size. We.We were also able to see that the filter
had high pressure drop,which resulted from the low porosity
due to the morphological change as shown in Fig. 9.