The parallelism control of the grinding procedure that removed layers of few micrometers was done with the aid of a previous indentation pattern on three points of the sample perimeter. The patterns were observed in an optical microscope (Zeiss Axiotech) and the thickness of each removed layer was calculated by geometrical means.