(Figure 4 (a),Table 2), which is in
accordance with the XRF and XRD analyses results. The
EDS profile of nanosilica particles (Figure 4 (b)) contained
(predominantly) the elements of Si and O with a molar ratio
of 1.8, which is very close to the stoichiometric ratio 2 of
natural silica.