OPT on the other hand show a ‘shoulder’ pattern, which is
caused by the amount of cellulose and hemicellulose in each type of biomass. It is noted that when the
temperature reaches 650°C, the degradation rates are no longer significant as most volatiles had already
been pyrolysed.