The degradation of cellulosic substances such as hemicellulose and cellulose in PALF started at about 225 oC,
followed by the decomposition of PLA, starting at 370 oC,
and the degradation of such composites completed at about 500 oC,
leaving char residue of 17-20 % depending on the amount of PALF