The N2 was used as carrier gas
were varied on 50, 100 and 200 ml/min, the pyrolysis temperature were as 300, 350, 400 and 450 C since
the results from TGA (Thermal gravimetric analysis) showed the same significantly weight loss
percentage of shell and residue between 300-450 C as showed in Fig.2.