This part is designed to obtain various aged pressboard samples with different DP values. Firstly, the new pressboard samples are prepared with the thickness of 1.5 mm and diameter of 136 mm and dried at 105 °C for 24 h in a vacuum (50 Pa) dry oven. Then these samples are taken out to absorb moisture in air until they reached a 0.5% moisture content