. Powdered samples were
mounted onto sample stage to record the crystallinity
index. Sample stage was mounted on horizontal axis and
the diffracted beam optics and the detector were mounted
on 2 axis. The scanning rate was 0.5°/min at 2 = 5° -
35° under the acceleration voltage of 30 KV and 20 mA.