The heat distortion temperature values suggested that the modified PLA could resist the thermal deformation from 58 C to a maximum value of 139 C when 1 lm talc was added at 10 wt%. With the presence of talc, the composites were more brittle and both tensile elongation at break and impact strength were decreased.