demonstrated the weight loss of individual raw materials with respect to temperature. Fig. 1e displayed total 19% weight loss related to removal of moisture, decomposition of hemicellulose, cellulose and lignin and the transformation of kaolinite to metakaolinite, confirmed by the DTA curve (Fig. 1f).