Then 20 g of samples were rinsed with tap water to remove dust and were subsequently soaked with
640 mL in 1,000 mL beaker. Next, 4 mL of CH3COOH, and 8 g of NaClO2 were added to the beaker for every hour for duration of 5 h where lignin was completely separated from fiber.