2.3.6. Mechanical properties
Mechanical tests were carried out using a TA-XT2i texture analyzer
(Surrey – England). The dimensions of film samples used in tests were
25 mm 100 mm, cut with sharp scissors. Prior to mechanical tests,
samples were conditioned at 25 C and 58% RH for 72 h.