After 10 days under ambient temperature, the highest level of TA (0.12%) was recorded in chitosan/nano-silica coated fruits, while the lowest value was found in untreated fruit (0.08%) followed by nano-silica composite (0.1%). This reason was probable that the nano-silica composite coating was unable to fine modify the internal atmosphere of the fruit to prevent the loss of TA contents.