Aqueous dispersion agents of vulcanising ingredients,
i.e., S, ZDEC and ZnO, were added to the latex at room temperature
with stirring at 200±20 rpm for 30 min. The mixture was left
for 2 h in a dark cabinet for maturation and was subsequently
heated in a water bath at 60 C.